You will love colored glaze at its first sight. It was considered as one of the seven kinds of treasure for Buddhists with a 2466 years’ history and as the first of Chinese Top-five famous wares. During the ancient times, it was exclusive for the imperial family and was so rare in the folk. In the legend the earliest cornucopia was made of colored glaze too, so it is considered as the keepsake of good fortune more direct and effective than the yellow quartz.
The current manufacturing technology of colored glaze, which has changed a lot over a long period of time compared to the previous times, is quite complicated, containing dozens of processes to finish. The making course of some fine works will take more than ten or twenty days, and depend on the hand mainly.
Each process needs elaborate treatment, controlling the duration and degree of heating half depends on luck and half on skills. Something more strictly, unlike gold and silver products, the colored glaze made by ancient method is not recoverable, that means a little flaw will spoil all efforts. So there are not two same pieces of colored glaze in the world.
The colored glaze is a kind of artistic works made of the artificial crystal, in the method of dewaxing & precisely casting. This course needs several dozen meticulous handcraft operations, and any slightly neglect will immediately result in the failure or flaws.
Characteristic of the works--It is tediously long to make the colored glaze, from the conception, the draft design, the sculpture of three-dimensional prototype, to the finish of the works, the whole course needs many strictly procedures and takes more than about two months.
The handicraft manufacture--To operate it, the workers must control the consummate technique. Each working procedure has its indefinite variety factor, and needs to be tested repeatedly in the process. None of their colors is identical. It is extremely difficult to make them.
Firing under a high temperature--The raw material should be melted into various kinds of colored crystal glass under a high temperature of more than 1400°C, and then after being carefully chosen and washed many times, it should be put into the mould according to the proportion. The furnace temperature must be controlled less than 1000 °C ±5 °C with the rising or dropping curve of the temperature being established strictly. The course of firing will last over 15 days to make the crystal materials precise in each detail, and then a piece of exquisite, three-dimensional, streamline works will be attained.
One mould for one piece--A mould can only be used to fire one piece of works. The large-scale complicated works even need to be molded and fired many times. The low success-rate makes the works more valuable. The works is issued in the whole world with quantity limitation, which makes each of the works more worthy of being collected.
(The above colored glaze pictures are offered by Daning Jewelry, for more information please click here.) |